Thermoplastic Polyolefin (TPO) roofing membranes are a popular choice in the construction industry for single-ply roofing systems due to their exceptional performance and durability. Produced using state-of-the-art AMUT facilities sourced from Italy, these TPO membranes are of the highest quality, meeting rigorous international standards.
The product has obtained CE and FM certifications, ensuring compliance with European and international safety and performance requirements. Notably, the TPO membrane boasts an artificial climate-accelerated aging time of 15,000 hours, significantly surpassing the national standard. This remarkable feature enhances the membrane's aging resistance, waterproofing capabilities, thermal insulation properties, and wind uplift resistance, making it a superior choice for various roofing applications.
CANLON, a leading manufacturer in the industry, stands out by producing both type G and GL TPO and PVC waterproof membranes. Their products exhibit clear competitive advantages over peers, particularly in dimensional stability, weather resistance, and wind uplift resistance, making them a preferred choice for high-performance roofing solutions.
Thickness(mm) | Width(m) | Length(m) | Color choice |
1.2 | 2.0 | 20 | white |
2.0 | 2.0 | 15 | |
2.5 | 2.0 | 10 | |
Remarks | Warranty: 10-20 years Other sizes or colors are designed based on requirements |
NO. | Item | Value | |||
Smooth one (Category H) |
Fiber fleece- backed (Category L) |
Reinforced with polyester scrim (Category P) | |||
1 | Thickness of resin attaching to embedded scrim/ mm ≥ | ---------- | ---------- | 0.4 | |
2 | Tensile property | Max tensile force / N/cm ≥ | ---------- | 120 | 250 |
Tensile strength/ MPa ≥ | 12.0 | ---------- | ---------- | ||
Elongation at break/ % ≥ | 500 | 250 | --------- | ||
3 | Dimensional variation after heating/ 100% ≤ | 2.0 | 1.0 | 0.5 | |
4 | Low temperature flexibility | -40ºC (no crack) | |||
5 | Impermeability | 0.3MPa, 2h , impermeable | |||
6 | Compression resistance | 0.5kg.m (no penetration) | |||
7 | Tear strength of overlapping / N/mm ≥ | 4.0 | 3.0 | ||
8 | Water absorption (70 ºC 168h) / % ≤ | 4.0 | |||
9 | Heat aging (80ºC) |
Time duration | 672h | ||
Appearance | No bubble, crack, delamination, or pinhole | ||||
Retention rate of max tensile force / % ≥ | ---------- | 90 | 90 | ||
Retention rate of tensile strength / % ≥ | 90 | ---------- | ---------- | ||
Retention rate of elongation at break/ % ≥ | 90 | 90 | ---------- | ||
Low temperature flexibility | -40ºC (no crack) | ||||
10 | Chemical resistance |
Appearance | No bubble, crack, delamination, or pinhole | ||
Retention rate of max tensile force / % ≥ | ---------- | 90 | 90 | ||
Retention rate of tensile strength/ % ≥ | 90 | ---------- | ---------- | ||
Retention rate of elongation at break/ % ≥ | 90 | 90 | ---------- | ||
Low temperature flexibility | -40ºC (no crack) | ||||
11 | Artificial Weathering |
Time duration | 1500hb) | ||
Appearance | No bubble, crack, delamination, or pinhole | ||||
Retention rate of max tensile force / % ≥ | ---------- | 90 | 90 | ||
Retention rate of tensile strength / % ≥ | 90 | ---------- | ---------- | ||
Retention rate of elongation at break / ≥ | 90 | 90 | ---------- | ||
Low temperature flexibility | -40ºC (no crack) |